3M 5491 PTFE Extruded Film Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5491 PTFE Extruded Film Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Backing; ASTM D3752
170 microns
6.70 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.2 MPa
5980 psi
ASTM D3759
Elongation at Break 200 %
200 %
ASTM D3759
Peel Strength 0.38347 kN/m
2.1875 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Adhesive Type Silicone
Appearance Gray