3M 6146 Kraft Medium Duty Reinforced Water Activated Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 6146 Kraft Medium Duty Reinforced Water Activated Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Medium Duty Reinforced Water Activated Tape 6146 Kraft is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and high tack water activated adhesive system.Information provided by 3M
Physical Properties Metric English Comments
Thickness 165 microns
6.50 mil
Caliper; ASTM D645
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 63.6 - 68.9 MPa
9220 - 9990 psi
Film Tensile Strength at Break, TD 26.5 - 31.8 MPa
3840 - 4610 psi
Descriptive Properties Value Comments
Adhesive Type High Tack, Water Activated, modified Starch Based Adhesive