3M 695 Riveters Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 695 Riveters Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Riveters Tape 695 is a zone-coated polyethylene film tape with a tack-free center “window” for use in holding aircraft rivets in place prior to and during riveting.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3752
76.2 microns
3.00 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.4 MPa
2670 psi
ASTM D3759
Peel Strength 0.1643 kN/m
0.9375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance White adhesive, yellow translucent film