Material Notes:
3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack and also bonds well to a variety of surfaces including LSE plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Adhesive
81.3 microns
3.20 mil
Liner
102 microns
4.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.2410 kN/m
1.375 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.3287 kN/m
1.875 pli
HDPE, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.3287 kN/m
1.875 pli
Rigid Vinyl, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Painted Metal, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
ABS, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.351 kN/m
2.00 pli
Polycarbonate, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.36156 kN/m
2.0625 pli
Polyester, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
HDPE, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Rigid Vinyl, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.6355 kN/m
3.625 pli
Polyester, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Painted Metal, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.8108 kN/m
4.625 pli
ABS, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Polypropylene, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
101 kN/m
576 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #300 Acrylic
Liner 43# Densified Kraft