Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7620/7890 White Vinyl Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7620/7890 White Vinyl Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack and also bonds well to a variety of surfaces including LSE plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
81.3 microns
3.20 mil
Liner
88.9 microns
3.50 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.8108 kN/m
4.625 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.877 kN/m
5.00 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.88746 kN/m
5.0625 pli
Polycarbonate, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.8984 kN/m
5.125 pli
Polypropylene, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.90937 kN/m
5.1875 pli
Polycarbonate, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.97511 kN/m
5.5625 pli
Stainless Steel, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Extended
79.0 °C
174 °F
Short Term, 24 hrs
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Short Term, 24 hrs
-40.0 °C
-40.0 °F
Extended
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #300 Acrylic
Liner 55# Densified kraft
Users viewing this material also viewed the following: