Material Notes:
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indoor weather-exposed applications. The termination assemblies consist of a tubular insulator high dielectric constant (Hi-K) stress control tube, conformable Hi-k stress controlling compound and built-in silicone top seal. The insulator is made of a new dark gray silicone rubber with advanced tracking resistance and hydrophobic properties.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.86 MPa
850 psi
Silicone Rubber Insulator; ASTM D412
10.3 MPa
1490 psi
High-K Stress Control Tube; ASTM D412
100% Modulus 0.000896 GPa
0.130 ksi
Silicone Rubber Insulator; ASTM D412
0.00110 GPa
0.160 ksi
High-K Stress Control Tube; ASTM D412
300% Modulus 0.00276 GPa
0.400 ksi
Silicone Rubber Insulator; ASTM D412
0.00345 GPa
0.500 ksi
High-K Stress Control Tube; ASTM D412
Electrical Properties Metric English Comments
Dielectric Constant 3.6

@Frequency 60.0 Hz
3.6

@Frequency 60.0 Hz
Silicone Rubber Insulator, 1000 V, 50% RH; ASTM D150
22

@Frequency 60.0 Hz
22

@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
25

@Frequency 60.0 Hz
25

@Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH, 100 mil; ASTM D150
Dielectric Strength 11.8 kV/mm

@Thickness 1.91 mm
300 kV/in

@Thickness 0.0750 in
Environmental Sealing Compound; ASTM D149
19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
Dissipation Factor 0.0030

@Frequency 60.0 Hz
0.0030

@Frequency 60.0 Hz
Silicone Rubber Insulator, 1000 V, 50% RH; ASTM D150
0.10

@Frequency 60.0 Hz
0.10

@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
0.90

@Frequency 60.0 Hz
0.90

@Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH; ASTM D150
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303