Peel Strength |
0.05478 kN/m |
0.3125 pli |
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.0877 kN/m |
0.500 pli |
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.131 kN/m |
0.750 pli |
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.175 kN/m |
1.00 pli |
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.175 kN/m |
1.00 pli |
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.1972 kN/m |
1.125 pli |
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.1972 kN/m |
1.125 pli |
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.219 kN/m |
1.25 pli |
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.219 kN/m |
1.25 pli |
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.219 kN/m |
1.25 pli |
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.219 kN/m |
1.25 pli |
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.2410 kN/m |
1.375 pli |
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.263 kN/m |
1.50 pli |
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.263 kN/m |
1.50 pli |
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.263 kN/m |
1.50 pli |
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.29582 kN/m |
1.6875 pli |
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.29582 kN/m |
1.6875 pli |
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.3287 kN/m |
1.875 pli |
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.3287 kN/m |
1.875 pli |
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.351 kN/m |
2.00 pli |
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.351 kN/m |
2.00 pli |
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.351 kN/m |
2.00 pli |
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.36156 kN/m |
2.0625 pli |
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.3725 kN/m |
2.125 pli |
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.38347 kN/m |
2.1875 pli |
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.38347 kN/m |
2.1875 pli |
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.38347 kN/m |
2.1875 pli |
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.40538 kN/m |
2.3125 pli |
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.4163 kN/m |
2.375 pli |
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.438 kN/m |
2.50 pli |
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.44921 kN/m |
2.5625 pli |
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.44921 kN/m |
2.5625 pli |
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.4602 kN/m |
2.625 pli |
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.47112 kN/m |
2.6875 pli |
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.47112 kN/m |
2.6875 pli |
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.5040 kN/m |
2.875 pli |
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.5040 kN/m |
2.875 pli |
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.51494 kN/m |
2.9375 pli |
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.51494 kN/m |
2.9375 pli |
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.55877 kN/m |
3.1875 pli |
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.570 kN/m |
3.25 pli |
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
0.570 kN/m |
3.25 pli |
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.657 kN/m |
3.75 pli |
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
0.6793 kN/m |
3.875 pli |
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.7231 kN/m |
4.125 pli |
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
|
0.745 kN/m |
4.25 pli |
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
0.745 kN/m |
4.25 pli |
Glass, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330 |
|
0.8108 kN/m |
4.625 pli |
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |