3M 7993MP Hi-Performance Acrylic 200MP

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7993MP Hi-Performance Acrylic 200MP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materials. It features exceptional shear strength and adhesion to high surface energy (HSE) plastics and metal surfaces.Single side spacers aid in the construction of membrane switch circuiry, i.e. to protect leads, hold domes in place, or build spacersInformation provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Polyester
50.8 microns
2.00 mil
Adhesive
Mechanical Properties Metric English Comments
Peel Strength 0.394 kN/m
2.25 pli
90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
0.394 kN/m
2.25 pli
90° Peel, PET/PET, Initial (20 mins); ASTM D3330
0.4163 kN/m
2.375 pli
90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
0.438 kN/m
2.50 pli
90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
0.5040 kN/m
2.875 pli
90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
0.55877 kN/m
3.1875 pli
90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
0.6793 kN/m
3.875 pli
90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
0.701 kN/m
4.00 pli
90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
0.745 kN/m
4.25 pli
90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
0.789 kN/m
4.50 pli
90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
0.86554 kN/m
4.9375 pli
90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
0.8984 kN/m
5.125 pli
90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 27.0 - 175 °C
2.50 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+15 ohm-cm
2.70e+15 ohm-cm
ASTM D257
Surface Resistance >= 5.60e+16 ohm
>= 5.60e+16 ohm
ASTM D257
Insulation Resistance 6.50e+12 ohm
6.50e+12 ohm
100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 2.77
2.77
ASTM D150
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Dissipation Factor 0.012
0.012
ASTM D150
Descriptive Properties Value Comments
Adhesive Type 200MP
Liner 94# PCK 7.0