3M 8402 Polyester Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 8402 Polyester Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyester Tape 8402 is a film tape with a silicone adhesive for composite bonding and splicing of many silicone coated papers and films.Information provided by 3M
Physical Properties Metric English Comments
Thickness 22.9 microns
0.900 mil
Backing; ASTM D3752
48.3 microns
1.90 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 87.6 MPa
12700 psi
ASTM D3759
Elongation at Break 100 %
100 %
ASTM D3759
Peel Strength 0.263 kN/m
1.50 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Descriptive Properties Value Comments
Adhesive Type Silicone
Appearance Translucent green