Material Notes:
The 3M cold Shrink Silicone Rubber 3/C Cable Breakout Boots 8560 Series are a series of open-ended molded silicone rubber sealing assemblies that are factory expanded and mounted on removable inner supporting plastic cores. They are supplied for filed installation in a pre-stretched condition. The supporting cores are removed after the seal has been positioned for installation around the breakout area of a 3/C (three conductor) cable. Core removal allows the silicone rubber boot to shrink down to a pre-determined diameter, creating an environmental enclosure for individual cable phase legs and overall cable jacket. The 3M Cold Shrink Silicone Rubber 3/C Cable Breakout boots 8560 Series are designed to protection the phase leg breakout area of 3/C medium voltage shielded power cable, from exposure to moisture, contamination, corrosion, ozone, ultra-violet radiation, physical contact and other hazards associated with 3/C termination operating environments. These can be used in conjunction with 3M Cold Shrink Silicone Rubber Termination assemblies and 3M Silicone Rubber RJS Series 3/C Phase Rejacketing Systems for 3/C shielded power cable termination applications.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.45 MPa
1370 psi
ASTM D412
Elongation at Break 780 %
780 %
ASTM D412
100% Modulus 0.000860 GPa
0.125 ksi
ASTM D412
Tear Strength Test 1.03
1.03
[MPa] Die B; ASTM D624 B
Electrical Properties Metric English Comments
Dielectric Strength 23.1 kV/mm

@Thickness 1.65 mm
587 kV/in

@Thickness 0.0650 in
Track Resistance 21600 sec
21600 sec
ASTM D2303/IEC 587