Material Notes:
3M™ Adhesive Transfer Tape 9437 with 3M™ Adhesive 100MP is designed for harsh environments such as automotive, aerospace and outdoor applications.Features:Excellent temperature and chemical resistance.Exceptional shear holding strength at elevated temperatures.Strong bond to metals and high surface energy plastics (e.g. ABS, polycarbonate).Polyester liner provides excellent die-cutting surfaceInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Peel Strength 0.18626 kN/m
1.0625 pli
Polypropylene, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
0.526 kN/m
3.00 pli
Stainless Steel, 20 Minute Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
0.79981 kN/m
4.5625 pli
Stainless Steel, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
1.3695 kN/m
7.8125 pli
Stainless Steel, Ultimate Bond, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month