Material Notes:
Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm have demonstrated benefits in specialized extrusion, and calendering processes. Features and BenefitsProcess targets: Extrusion and processing of wire and cable, fiber spinning, and certain calendering operationsBroadens extrusion processing capabilities of certain types of polyolefin resinsExcellent thermal stabilityEffective as a process aid over a broad process temperature rangeFree flowing granular product form100% activeReduces/eliminates die build-upLowers apparent melt viscosityFor use at very low levelsCan offer performance and cost advantagesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.90 - 1.96 g/cc
1.90 - 1.96 g/cc
Particle Size <= 2400 µm
<= 2400 µm
0.98
Melt Index of Compound 15 - 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
15 - 25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
Thermal Properties Metric English Comments
Melting Point 110 - 126 °C
230 - 259 °F
Descriptive Properties Value Comments
Active Ingredients (%) 100
Color Clear to off-white
Form Free-flowing granular