3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Oxygen Transmission 98.0 cc-mm/m²-24hr-atm
249 cc-mil/100 in²-24hr-atm
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Modulus of Elasticity 0.140 GPa
20.3 ksi
Youngs Modulus
Coefficient of Friction, Dynamic 0.80
0.80
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
DSC
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
Dielectric Constant 11.4

@Frequency 6.00e+7 Hz
11.4

@Frequency 6.00e+7 Hz
Dielectric Strength 25.0 kV/mm