Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.5%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 70.5% F grade terpolymer with best permeation resistance to auto fluids. Gives smooth extrudates without process aids. Can be compounded to pass -40°C mandrel flex test. Used in Hose/Extrusion Applications.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Mooney Viscosity 33

@Temperature 121 °C
33

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Tensile Strength, Yield 4.40 MPa
638 psi
M100
Elongation at Break 250 %
250 %
Coefficient of Friction, Dynamic 0.80
0.80
Compression Set 44 %

@Temperature 200 °C
44 %

@Temperature 392 °F
70 hr; ASTM D395B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -7.00 °C
19.4 °F
TR10