3M Dyneon™ Fluorel™ FT-2320 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ FT-2320 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69% F grade terpolymer for difficult extrusions. Suggested alternative: FE-5730Q or FE-5830Q. Used in Hose/Extrusion Applications.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
Tensile Strength, Ultimate 14.0 MPa
2030 psi
Tensile Strength, Yield 5.20 MPa
754 psi
M100
Elongation at Break 230 %
230 %
Coefficient of Friction, Dynamic 0.80
0.80
Compression Set 39 %

@Temperature 200 °C
39 %

@Temperature 392 °F
70 hr; ASTM D395B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -12.0 °C
10.4 °F
TR10