Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.21 g/cc
0.0798 lb/in³
ASTM D4894
Apparent Bulk Density 0.820 g/cc
0.0296 lb/in³
ASTM D4894
Particle Size 800 µm
800 µm
ASTM D4894
Deformation 4.0 %

@Pressure 15.00 MPa
4.0 %

@Pressure 2175 psi
ASTM D621
6.0 %

@Time 86400 sec,
Pressure 15.00 MPa
6.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Initial; ASTM D2240
57

@Time 15.0 sec
57

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
ASTM D4894
Elongation at Break 375 %
375 %
ASTM D4894
Tensile Modulus 0.0965 GPa
14.0 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 30.0 - 100 °C
31.7 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
77.0 µm/m-°C

@Temperature 100 - 200 °C
42.8 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
95.0 µm/m-°C

@Temperature 200 - 300 °C
52.8 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.260 W/m-K

@Temperature 100 °C
1.80 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
0.270 W/m-K

@Temperature 250 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
Shrinkage 2.2 %
2.2 %
ASTM D4894