3M Dyneon™ TFM™ 1600 Modified PTFE Powder  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TFM™ 1600 Modified PTFE Powder  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generation PTFE, but with a significantly lower melt viscosity giving better particle fusion during sintering and smoother surfaces.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.165 g/cc
0.07822 lb/in³
ASTM D4894
Apparent Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894
Particle Size 4450 µm
4450 µm
ASTM D4894
Deformation 2.0 %

@Pressure 15.00 MPa
2.0 %

@Pressure 2175 psi
Permanent; ASTM D621
3.0 %

@Time 86400 sec,
Pressure 15.00 MPa
3.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
Initial; ASTM D2240
11

@Time 3600 sec
11

@Time 1.00 hour
58

@Time 15.0 sec
58

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 31.7 MPa
4600 psi
ASTM D4894
Elongation at Break 650 %
650 %
ASTM D4894
Tensile Modulus 0.650 GPa
94.3 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 30.0 - 100 °C
31.7 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
75.0 µm/m-°C

@Temperature 100 - 200 °C
41.7 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
92.0 µm/m-°C

@Temperature 200 - 300 °C
51.1 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.230 W/m-K

@Temperature 100 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
0.240 W/m-K

@Temperature 250 °C
1.67 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
Shrinkage 3.5 %
3.5 %
ASTM D4894
Electrical Properties Metric English Comments
Dielectric Strength 2.60 kV/mm
66.0 kV/in
ASTM D149