3M FM02511K Clear Laser Imprintable Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FM02511K Clear Laser Imprintable Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Clear Laser Imprintable Label Product FM02511K is a durable high performance material that offers excellent thermal stability and moisture resistance. This product is suitable for demanding applications such as nameplates and product ID labels. This polyester label utilizes 3M™ P1400, which is a high performance tackified acrylic designed for use in demanding environments.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Facestock
150 microns
5.90 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.386 kN/m
2.20 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
125 °C
257 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1400 Perm. 18
Liner 83# Laser