Material Notes:
3M™ White Polypropylene Label Product FP027202 is a glossy white opaque material that offers excellent durability and moisture resistance. This label product utilizes 3M™ Adhesive P1400, which is a high performance tackified acrylic designed for use in demanding environments.Information provided by 3M
Physical Properties Metric English Comments
Thickness 58.4 microns
2.30 mil
Facestock
78.7 microns
3.10 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.386 kN/m
2.20 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1400 Perm 0.9
Liner 50# SC