3M Jet-Weld™ TS-230 Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer 3M
Trade Name Jet-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Jet-Weld™ TS-230 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Sprayable/extrudable grade with long set time ideal for bonding a wide variety of plastics, including polystyrene and polyacrylic. Can bond aluminum and glass to plastic and wood. The color is white/off white. The open time is 4 minutes, and the set time is 2.5 minutes.Information provided by 3M Adhesives Division.
Physical Properties Metric English Comments
Viscosity 9000 cP
9000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
Tensile Strength, Ultimate 22.8 MPa
3310 psi
Elongation at Break 700 %
700 %
Modulus of Elasticity 0.0372 GPa
5.40 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Processing Temperature 121 °C
250 °F