3M Scotch® 232 High Performance Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 232 High Performance Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® High Performance Masking Tape 232 is designed to be used in medium temperature paint bake operations.Information provided by 3M
Physical Properties Metric English Comments
Thickness 4.06 microns
0.160 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.5 MPa
4280 psi
ASTM D3759
Elongation at Break 8.0 %
8.0 %
ASTM D3759
Peel Strength 0.29582 kN/m
1.6875 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
for 30 mins
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Tan