3M Scotch® 3311 Foil Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 3311 Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Foil Tape 3311 is an aluminum alloy foil with a pressure-sensitive adhesive and paper liner. The aggressive rubber adhesive sticks well to most surfaces and the paper liner makes for convenient and reliable use.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing
91.4 microns
3.60 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.1 MPa
4800 psi
ASTM D3574
Elongation at Break 3.0 %
3.0 %
ASTM D3759
Peel Strength 0.9861 kN/m
5.625 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Application
82.2 °C
180 °F
Minimum Service Temperature, Air -23.3 °C
-9.94 °F
-12.2 °C
10.0 °F
Application
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Silver