3M Scotch® 35 Vinyl Electrical Tape

Category Polymer , Tape , Thermoplastic , Vinyl (PVC)
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 35 Vinyl Electrical Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identification, color coding of motor leads and piping systems, and for marking safety areas. Scotch® Tape 35 operates over a wide range of temperatures-up to 105°C; applies smoothly and conforms well above 0°C. This tape is available in nine fade resistant colors.Information provided by 3M
Physical Properties Metric English Comments
Thickness 178 microns
7.00 mil
Mechanical Properties Metric English Comments
Elongation at Break 225 %
225 %
ASTM D1000
Peel Strength 0.219 kN/m
1.25 pli
Adhesion to Steel; ASTM D1000
0.219 kN/m
1.25 pli
Adhesion to Backing; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air 0.000 °C
32.0 °F
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D1000
Dielectric Strength 49.2 kV/mm
1250 kV/in
Dielectric Breakdown 7875 V
7875 V
Wet Condition (96 hrs @ RT); ASTM D1000
8750 V
8750 V
Standard condition; ASTM D1000
Descriptive Properties Value Comments
Appearance Blue, Brown, Gray, Green, Orange, Red, Violet, White, Yellow