3M Scotch® 375 Superior Performance Box Sealing Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 375 Superior Performance Box Sealing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Box Sealing Tape 375 is a superior performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. The product has the strongest conformable backing and the most consistent pressure sensitive hot melt adhesive system available. This time proven construction assures superior performance in a wide range of environments and applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
78.7 microns
3.10 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 7.76 MPa
1130 psi
ASTM D3759
Film Tensile Strength at Break, TD 15.5 MPa
2250 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive hot melt rubber-resin
Appearance Clear and tan