3M Scotch® 828 Custom Printed Pouch Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 828 Custom Printed Pouch Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A pressure sensitive pouch tape printed tape with a company logo or design in a variety of colors. This tape features a clear, non-tacky window for displaying documents and it offers a strong Scotchpro™ film backing which is coated with an aggressive adhesive to provide excellent adhesion to a wide range of boxes.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.5478 kN/m
3.125 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 0.795 MPa
115 psi
ASTM D3759
Film Tensile Strength at Break, TD 1.59 MPa
231 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure Sensitive Rubber Resin
Appearance Red, Blue, Green, Yellow, Orange, and Black