3M Scotch-Seal™ 1252 Tamper Proof Sealant

Category Polymer
Manufacturer 3M
Trade Name Scotch-Seal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Seal™ 1252 Tamper Proof Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustment or other evidence of tampering by a break in the seal when the part is altered in position. Has been effectively used in the electronics industry to protect settings and calibrations of electronic equipment against tampering, to seal electronic components between stages of assembly, to aid in the visual inspection of subassembly components, equipment and parts which are restricted to adjustment, alteration, or access by qualified personnel. Exposed surfaces will accept ink from an inspector’s approval stamp and can be marked as soon as 20 seconds after the sealer application.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 61 - 73 %
61 - 73 %
Brookfield Viscosity 500 - 2500 cP
500 - 2500 cP
RVF #6 sp. @ 4 rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 97 - 99

@Time 86400 sec
97 - 99

@Time 24.0 hour
50% RH
Shear Strength 1.13 MPa
164 psi
Overlap, Steel
1.19 MPa
173 psi
Overlap, Aluminum
Thermal Properties Metric English Comments
Flash Point -4.00 °C
24.8 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+10 ohm-cm
>= 1.00e+10 ohm-cm
Surface Resistance >= 1.00e+10 ohm
>= 1.00e+10 ohm
Dielectric Strength >= 3.94 kV/mm
>= 100 kV/in
Processing Properties Metric English Comments
Shelf Life 9.00 - 12.0 Month
9.00 - 12.0 Month