Flexible and Conveyor belt repairInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 100000 cP
100000 cP
Mechanical Properties Metric English Comments
Shear Strength 4.14 MPa
600 psi
Processing Properties Metric English Comments
Cure Time 15.0 min
0.250 hour
Time to Handling Strength