Material Notes:
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, metals, and other common substrates. They are available in a wide variety of viscosities. Slow cure for porous material or gap filling. It is also used on assemblies where parts are not close-fitting, surfaces are rough or porous, or where time is required to align parts before cure.Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Uncured
Viscosity 2500 cP
2500 cP
Brookfield Viscosity 2175 - 2750 cP
2175 - 2750 cP
LVF sp #3 @30 rpm
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
cured; ISO 6922
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.333 - 1.00 min
0.00555 - 0.0167 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear liquid