Material Notes:
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG05 PR is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates or in combination with meal or composite substrates. Scotch-Weld Medical Grade Instant Adhesive MG05 PR is recommended for use on assemblies with very close-fitting parts and can be used to wick into bonding gaps of assembled parts.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 2.0 - 6.0 cP
2.0 - 6.0 cP
ISO 3104/3105
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
cured, grit-blasted steel; ASTM D2095
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0167 - 0.167 min
0.000278 - 0.00278 hour
Time to Handling
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid