Material Notes:
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG1500 PR is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates or in combination with meal or composite substrates. The high viscosity of MG1500 PR gives it greater gap-filling capabilities and it will not wick into unwanted areas.Information provided by 3M
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Brookfield Viscosity 1275 - 1650 cP
1275 - 1650 cP
LVF, sp 3 @ 30 rpm
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 MPa
5000 psi
cured, grit-blasted steel; ASTM D2095
Shear Strength 19.3 MPa
2800 psi
Overlap, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.333 - 1.67 min
0.00555 - 0.0278 hour
Time to Handling
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid