3M Scotch-Weld™ TL22 Threadlocker Anaerobic Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ TL22 Threadlocker Anaerobic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening and/or leakage. All products provide excellent vibration, corrosion, and shock resistance. Engineered to provide different strengths, temperatures, nut/bolt sizes, and other requirements, some threadlockers allow removal and meet various selections depending on the specific application. TL22 is removable with hand tools. It is a low strength (low torque removal) threadlocker for small diameter, fine threaded screws, set screws, nuts, bolts, hex and slot driven components such as keyed fasteners.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 800 - 1600 cP
800 - 1600 cP
RVT #3 sp @ 20 rpm
Processing Properties Metric English Comments
Cure Time <= 5.00 min
<= 0.0833 hour
Fixture Time with Activator
<= 20.0 min
<= 0.333 hour
Fixture Time
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Purple