3M Scotchkote™ 80BG 536 Urethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 80BG 536 Urethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties similar to factory produced rubbersDesigned for application by trowel or spatula at thicknesses up to 500 micronsPrimarily designed for use to resurface impellers, chutes, and hoppers.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Thickness 508 microns
20.0 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength at Break 11.7 MPa
1700 psi
Elongation at Break 600 %
600 %
Electrical Properties Metric English Comments
Dielectric Strength 16.0 kV/mm
406 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Initial Set
960 min
16.0 hour
Machining Time
1440 min
24.0 hour
Full Mechanical
Descriptive Properties Value Comments
Appearance Black