3M Scotchkote™ GP 120 Epoxy Primer

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ GP 120 Epoxy Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.Product Features:Suitable for use on mechanically prepared steelwork or high pressure water cleaned steel, can also be used on abrasive blasted steel.Can be applied over existing coatings.Can be used as a two coat primer/finish system or overcoated with a variety of top coats. Information provided by 3M
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Solids Content 90 %
90 %
Volatile Organic Compounds (VOC) Content 83 g/l
83 g/l
Thickness 3180 microns
125 mil
Dry
3560 microns
140 mil
Wet
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
Touch Dry
1440 min
24.0 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Silver