Material Notes:
Scotchkote Urethane Metal Repair RG 501 has been specifically developed as a rapid curing repair system for rebuilding and repairing equipment requiring good mechanical strength.Product Features:Combines good application characteristics with speed of cure to minimize down timeDesigned for application by putty knife or spatula at thicknesses up to 6 mmCan be applied to any damaged metal surface, plus glass, fiberglass and other composite surfacesDesigned for rapid repairs to cracked casting, leaking pipes, tanks and flangesExhibits excellent adhesion to correctly prepared metal surfaces. Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 6100 microns
240 mil
Mechanical Properties Metric English Comments
Flexural Strength 49.0 MPa
7100 psi
Compressive Strength 84.1 MPa
12200 psi
Shear Strength 17.2 MPa
2500 psi
Tensile Shear Adhesion, on a grit blasted steel
Thermal Properties Metric English Comments
Heat Distortion Temperature 52.0 °C
126 °F
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
Initial Set
30.0 min
0.500 hour
Hard Dry for machining
120 min
2.00 hour
Full Mechanical
Descriptive Properties Value Comments
Appearance Gray