3M Scotchkote™ SP 810 Epoxy Sealer

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ SP 810 Epoxy Sealer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Sealer SP 810 has been specifically developed as a low viscosity primer/sealer for concrete and cementitious surfaces prior to application of other Scotchkote 100% solids epoxy system.Product Features:Combines good application characteristics with excellent penetration and adhesionDesigned for application by brush or rollerDesigned for use on concrete surfaces but can be used on other porous mineral substrates Information provided by 3M
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Solids Content 100 %
100 %
Thickness 102 microns
4.00 mil
Processing Properties Metric English Comments
Cure Time 120 min
2.00 hour
Touch Dry
960 min
16.0 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear