Material Notes:
3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (MRO), general Industrial and transportationCaulking, sealing and gap fillingInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 79 - 84 %
79 - 84 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.48 MPa
215 psi
0.758 MPa

@Temperature 121 °C
110 psi

@Temperature 250 °F
0.896 MPa

@Temperature 71.0 °C
130 psi

@Temperature 160 °F
0.896 MPa

@Temperature 93.0 °C
130 psi

@Temperature 199 °F
0.931 MPa

@Temperature 49.0 °C
135 psi

@Temperature 120 °F
1.00 MPa

@Temperature 60.0 °C
145 psi

@Temperature 140 °F
1.59 MPa

@Time 605000 sec
231 psi

@Time 168 hour
180°F (82°C) and then tested at 75°F (24°C)
1.62 MPa

@Time 1.21e+6 sec
235 psi

@Time 336 hour
180°F (82°C) and then tested at 75°F (24°C)
1.65 MPa

@Time 2.59e+6 sec
239 psi

@Time 720 hour
180°F (82°C) and then tested at 75°F (24°C)
1.69 MPa

@Time 5.18e+6 sec
245 psi

@Time 1440 hour
180°F (82°C) and then tested at 75°F (24°C)
Elongation at Break 160 %
160 %
110 %

@Temperature 121 °C
110 %

@Temperature 250 °F
130 %

@Temperature 93.0 °C
130 %

@Temperature 199 °F
150 %

@Temperature 71.0 °C
150 %

@Temperature 160 °F
165 %

@Temperature 60.0 °C
165 %

@Temperature 140 °F
175 %

@Temperature 49.0 °C
175 %

@Temperature 120 °F
150 %

@Time 1.21e+6 sec
150 %

@Time 336 hour
180°F (82°C) and then tested at 75°F (24°C)
150 %

@Time 5.18e+6 sec
150 %

@Time 1440 hour
180°F (82°C) and then tested at 75°F (24°C)
175 %

@Time 2.59e+6 sec
175 %

@Time 720 hour
180°F (82°C) and then tested at 75°F (24°C)
175 %

@Time 605000 sec
175 %

@Time 168 hour
180°F (82°C) and then tested at 75°F (24°C)
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month