Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

5265 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 5265 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D412
Tensile Strength, Yield 22.8 MPa
3300 psi
at 100%; ASTM D412
Elongation at Break 460 %
460 %
ASTM D412
Tear Strength 210 kN/m
1200 pli
die B; ASTM D624
Compression Set 20 %
20 %
ASTM D395
Copyright © lookpolymers.com All Rights Reserved