A. Schulman ComAlloy Hiloy® 125 Polypropylene, Glass Reinforced, Chemically Coupled

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 125 Polypropylene, Glass Reinforced, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
298 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C