A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 103 MPa
14900 psi
ASTM D638
Elongation at Break 4.4 %
4.4 %
ASTM D638
Flexural Strength 158 MPa
22900 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 227 °C
441 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F