Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 152 MPa
22000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 216 MPa
31300 psi
ASTM D790
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.95 J/cm
7.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 280 - 290 °C
536 - 554 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
Users viewing this material also viewed the following: