Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 101 MPa
14600 psi
ASTM D638
Elongation at Break 6.6 %
6.6 %
ASTM D638
Flexural Strength 149 MPa
21600 psi
ASTM D790
Flexural Modulus 8.70 GPa
1260 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.86 J/cm
9.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 - 268 °C
496 - 514 °F
Deflection Temperature at 0.46 MPa (66 psi) 202 °C
396 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
Copyright © lookpolymers.com All Rights Reserved