A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy

Category Polymer , Thermoplastic , Ionomer , Nylon
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. ApplicationFormion® FI 200 is targeted for non painted, mold-in -color, exterior or interior appearance applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
ISO 527
Elongation at Break 270 %
270 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75