Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0070 - 0.011 cm/cm

@Thickness 3.20 mm
0.0070 - 0.011 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
0.0060 - 0.010 cm/cm

@Thickness 3.20 mm,
Time 259000 sec
0.0060 - 0.010 in/in

@Thickness 0.126 in,
Time 72.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.0 MPa
6090 psi
at max load; ISO 527
Elongation at Break 225 %
225 %
ISO 527
Flexural Modulus 2.44 GPa
354 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Izod Impact, Unnotched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C

@Thickness 3.17 mm
214 °F

@Thickness 0.125 in
ISO 75