Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.010 - 0.014 cm/cm

@Thickness 3.20 mm
0.010 - 0.014 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
15 sec delay; ISO 868
Tensile Strength, Ultimate 16.0 MPa
2320 psi
at max load; ISO 527
Elongation at Break 425 %
425 %
ISO 527
Flexural Modulus 0.430 GPa
62.4 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 38.0 °C

@Thickness 3.20 mm
100 °F

@Thickness 0.126 in
ISO 75