A. Schulman FORMION™ FI 372 Ionomer

Category Polymer , Thermoplastic , Ionomer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman FORMION™ FI 372 Ionomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm

@Thickness 3.20 mm,
Time 259000 sec
0.0060 - 0.010 in/in

@Thickness 0.126 in,
Time 72.0 hour
ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
15 sec delay; ISO 868
Tensile Strength, Ultimate 24.0 MPa
3480 psi
at max load; ISO 527
Elongation at Break 95 %
95 %
ISO 527
Flexural Modulus 1.03 GPa
149 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C

@Thickness 3.17 mm
115 °F

@Thickness 0.125 in
ISO 75