Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
15 sec delay; ISO 868
Tensile Strength, Ultimate 24.0 MPa
3480 psi
at max load; ISO 527
Elongation at Break 20 %
20 %
ISO 527
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) 63.0 kJ/m²
30.0 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C

@Thickness 3.20 mm
117 °F

@Thickness 0.126 in
ISO 75