A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and excellent weatherability. ApplicationInvision™ VX-5170UE is targeted for profile and sheet extrusion appearance and functional applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183/1
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
15 sec delay; ISO 868
Tensile Strength at Break 4.90 MPa
711 psi
ISO 527
Tensile Strength, Yield 3.30 MPa

@Strain 100 %
479 psi

@Strain 100 %
ISO 527
Elongation at Break >= 350 %
>= 350 %
ISO 527
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
Descriptive Properties Value Comments
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)
SAE J1885