Material Notes:
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low temperature toughness. ApplicationInvision™ VX-6060UE is targeted for automotive extrusion appearance applications. Information provided by A. Schulman.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 sec delay; ASTM D2240
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Tensile Modulus 0.00270 GPa
0.392 ksi
2% Secant, 500 mm/min; ASTM D638
0.0147 GPa
2.13 ksi
100% Secant, 500 mm/min; ASTM D638
Flexural Modulus 0.0139 GPa
2.02 ksi
1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790
Descriptive Properties Value Comments
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)
SAE J1885