Material Notes:
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-01 meets FDA Regulation 21 CFR 177.1520(c) 3.1 and 3.2.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ASTM D792
ESCR 100% Igepal® 5.0 hour
5.0 hour
Condition B; ASTM D1693
Melt Index of Compound 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 22.8 MPa
3300 psi
2"/min; ASTM D638
Elongation at Break 100 %
100 %
2"/min; ASTM D638
Flexural Modulus 0.793 GPa
115 ksi
1% secant; ASTM D882
Izod Impact, Notched >= 0.534 J/cm
>= 1.00 ft-lb/in
ASTM D256
Falling Dart Impact 32.5 J
24.0 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746