Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
16900 psi
ASTM D638
Flexural Strength 180 MPa
26100 psi
ASTM D790
Flexural Modulus 7.93 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm
16.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 117 °C
243 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 130 °C
266 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying